Closed for Thanksgiving week (Nov 23–29). We are still answering calls, texts and email, but no orders are being built, worked on or shipped until we are back on Monday, Nov 30. If timing matters or you would rather cancel, just ask: a full refund is no problem, no pressure. It has been a very busy two months. Thank you for your patience. — Kevin, 415.341.2281, 11/25
BeeLatch: still catching up on backorders, shipping in the order they came in · Updated Sun, Nov 15, 2026 · details
EMGElectric Moto GarageConnected motorcycle tech
Write-up · Battery tech

Lithium dendrites: why e-moto batteries catch fire

Tiny metal spikes grow inside lithium cells when they are charged cold, fast or after sitting dead. Here is how one spike turns into a fire, in plain English, and what you can do about it.

By Kevin Graehl, Electric Moto Garage · San Francisco · November 2026

TL;DR

  • Dendrites are tiny spikes of lithium metal that grow inside a cell when it is charged in a way the cell can't keep up with: too fast, too cold, too full, or after the pack has been run far too low.
  • They grow slowly and you can't see them. A pack can look and ride perfectly fine until a spike pokes through the thin plastic wall (the separator) between the two sides of the cell.
  • That makes an internal short. The short heats one spot, the heat melts more of the wall, and the cell can go into thermal runaway: it heats itself, vents flammable gas and catches fire.
  • Normal lithium-ion cells carry their own fuel and their own oxygen, so the fire is very hard to put out and can spread cell to cell through a whole pack.
  • LFP and solid-state cells lower the risk, but not to zero.
  • Any battery with a cell that went below 2 V gets recycled. Bypassing the BMS to force a charge feeds the dendrites already growing inside. Why there are no excuses →
  • Biggest things you control: don't charge a cold pack, don't charge a pack that sat dead without a check, and use a proper charger. A pack that sat dead is how many of these start. See why a parked SURRON battery drains so low →
  1. What is inside a lithium cell
  2. What a dendrite is
  3. What makes dendrites grow
  4. From spike to fire, step by step
  5. Two easy ways to picture it
  6. LFP and solid-state: safer, not fireproof
  7. Below 2 V a cell? Recycle it
  8. What riders can do
  9. Sources

What is inside a lithium cell

Every lithium-ion cell in your SURRON, e-bike or electric unicycle (EUC) pack has the same basic parts:

  • The anode (negative side), usually graphite on a copper foil.
  • The cathode (positive side), a metal oxide such as NMC or a phosphate such as LFP, on aluminum foil.
  • The separator, a plastic film thinner than a sandwich bag that keeps the two sides from touching.
  • The electrolyte, a liquid that soaks everything and lets lithium ions travel between the sides.

When you charge, lithium ions leave the cathode, cross the separator and slide into the graphite, like cars pulling into parking spaces. When you ride, they drive back out.

What a dendrite is

If ions arrive faster than the graphite can take them in, they can't park. Instead they pile up on the surface as solid lithium metal. This is called lithium plating. Plated lithium does not spread out smooth and even. It grows in spiky, branching, moss-like whiskers. Those whiskers are dendrites.

A dendrite (gold) grows from the anode, pushes through the separator and touches the cathode. That contact is an internal short circuit. Simplified drawing, not to scale.

What makes dendrites grow

Charging cold

This is the big one for riders. Below about 0 °C (32 °F), graphite takes in lithium very slowly, so even a normal charge rate can plate. Plugging in a frozen bike straight after a winter ride is the classic way it happens.

Charging too fast

High current pushes ions in faster than the anode can absorb them, most of all near the end of the charge.

Overcharging or sitting full

A nearly full anode has few open parking spots left. A wrong or faulty charger that pushes past the pack's full voltage makes it much worse.

Over-discharge, then recharge

Run a cell far below its safe minimum and the copper foil on the anode can start to dissolve. When you charge again, the copper comes back as conductive spikes. That is why a pack that has sat dead for months has to be checked cell by cell before it is charged.

Age and wear

As the anode wears out it gets worse at taking in lithium, so plating starts at lower charge rates than when the cell was new.

Factory defects

A metal burr, a speck of dust or a wrinkle in the separator is a ready-made weak spot. This is a common way cheap, poorly checked cells fail.

From spike to fire, step by step

  1. Pierce. The dendrite grows through the separator. One research review puts the danger point at roughly 10 micrometres, which is enough to push through a common plastic separator.
  2. Short. The two sides of the cell now touch through a tiny metal bridge. Current dumps through that one spot and heats it fast.
  3. Melt. The heat melts more of the separator, which makes the short bigger, which makes more heat. It feeds itself.
  4. Thermal runaway. Somewhere between about 130 °C and 250 °C or more (it depends on the cell), the chemistry starts making its own heat. The liquid electrolyte is a flammable solvent, and most high-energy cathodes (NMC and NCA) release oxygen as they break down. The cell vents hot, flammable gas, often as a jet of flame.
  5. Spread. One cell burning at several hundred degrees cooks the cells touching it. In an e-moto pack with dozens or hundreds of cells, that turns into a chain reaction.
Why it is so hard to put out: an ordinary fire needs air, so you can smother it. A burning NMC cell brings its own oxygen. A lid, a blanket or a bucket of sand won't stop it, and it can flare back up after it looks finished. If a pack is smoking or hissing, get away from it, get people out and call 911.

Two easy ways to picture it

🧊 The icicle through the screen door

The separator is a thin screen door between two rooms that must never touch. Charge too hard, or charge cold, and lithium freezes onto the anode as icicles instead of going inside. Each charge makes them a little longer. One day an icicle pokes through the screen, the rooms touch, and the house goes up. It happens slowly, over many charges, and you can't see it from the outside.

🔥 The campfire in a sealed can

A normal campfire needs air. A burning lithium cell is a can of lighter fluid (the electrolyte) packed with oxygen tablets (the cathode). Once it is lit it feeds itself, and closing the lid does nothing. It burns until the fuel is gone, then lights the next can over.

LFP and solid-state: safer, not fireproof

NMC / NCA (most e-moto and EUC packs)LFP (lithium iron phosphate)Solid-state
ElectrolyteFlammable liquidFlammable liquidSolid, much less fuel
Oxygen from the cathodeYes, feeds the fireVery littleDepends on the cathode
Runaway startsLower temperatureHigher temperatureStill being proven
Can grow dendrites?YesYesYes, through cracks and grain boundaries
TradeoffMost energy for its weightHeavier and bulkier for the same rangeMostly not in rider products yet

LFP holds on to its oxygen, starts runaway at a higher temperature, burns cooler and throws out far less material. It still uses a flammable electrolyte and still vents flammable gas, so it is harder to light and gentler when it does burn, but it can still burn. That extra weight is why most high-performance bikes and wheels still use NMC-type cells.

Solid-state swaps the liquid for a solid, which removes the biggest fuel source. Dendrites can still grow through solid electrolytes, and many designs pair them with pure lithium-metal anodes. They are promising, but a "solid-state" label on a spec sheet is not a safety guarantee by itself.

Below 2 V a cell? Recycle it. No excuses.

Yes, you can open a SURRON battery, bypass the BMS and force a charge into cells that dropped below 2 volts. The pack may even take the charge and look fine for a while. Please don't be tempted.

  • The damage has already started. Once a cell has been below 2 V, and often even below 2.5 V, dendrites have started forming inside it. Recharging feeds them.
  • There is no way to know how many. Nobody can see inside a sealed cell. Not us, not a meter, not a charger.
  • Your fire risk goes up enormously. Every spike is a possible internal short, and charging is when they grow.
  • It may heat up when you charge it, because those cells are already damaged.
  • Your range will suffer. The capacity those cells lost doesn't come back.

Our rule: any battery with a cell below 2 V gets recycled. No excuses. Don't throw it in the trash. Take it to a battery recycler. In the US, Call2Recycle's locator finds drop-off points. Not sure how low yours went? We check it cell by cell first.

What riders can do

  • Don't charge a cold pack. Bring the bike or battery inside and let it warm to room temperature first.
  • Use the right charger. It must match your pack's voltage and connector. Not sure which plug you have? See the SURRON charging connector guide.
  • Don't let a pack sit dead. Keep a parked bike topped up to 60 to 80% each month. Here is why a parked SURRON battery keeps draining.
  • Never bypass the BMS to charge a pack that went below 2 V a cell. Recycle it.
  • Get a dead pack checked before charging it. What to do if your SURRON battery won't charge.
  • Charge where you'd notice smoke, away from your only exit and away from anything that burns easily.
  • Treat damage seriously. A pack that was dropped hard, got wet, swelled up or runs hotter than usual should be inspected, not just plugged back in.

Sources

Exact temperatures vary a lot from cell to cell and source to source, so treat the numbers here as ballpark figures. The overall picture (NMC-type cells go into runaway sooner and burn hotter than LFP) is the same in every source.

FAQ

Questions

What is a lithium dendrite?

A tiny spike of lithium metal that grows on the anode when lithium ions arrive faster than the graphite can take them in. It grows a little with each bad charge, and you can't see it from outside the cell.

Why do dendrites cause battery fires?

A dendrite can grow through the thin plastic separator and touch the other side of the cell. That internal short heats one spot, melts more separator and can start thermal runaway, where the cell heats itself and vents flammable gas.

Is it bad to charge an e-bike or SURRON battery in the cold?

Yes. Below about 0 °C (32 °F) the anode takes in lithium very slowly, so normal charging can plate lithium metal and grow dendrites. Let the battery warm to room temperature before you charge it.

Is it safe to charge a lithium battery that has been dead for months?

Not without a check. Cells that drop far below their safe minimum can dissolve copper inside, which comes back as conductive spikes when charged. Have the pack checked cell by cell first.

Can I bypass the BMS and charge a SURRON battery that went below 2 V a cell?

Please don't. Once a cell has been below 2 V, and often even below 2.5 V, dendrites have started forming, and there is no way to know how many. Charging it raises the fire risk enormously, it may heat up while charging, and the range will suffer. Recycle any battery with a cell below 2 V. No excuses.

Are LFP batteries fireproof?

No. LFP starts thermal runaway at a higher temperature, releases very little oxygen and burns cooler, but it still uses a flammable liquid electrolyte and can still vent flammable gas.

Do solid-state batteries stop dendrites?

Not completely. They remove most of the flammable liquid, but dendrites can still grow through cracks and grain boundaries in a solid electrolyte. They lower the risk rather than remove it.